The concentrate entering the sintering stage carries 1.40 per cent lithium and 0.98 per cent rubidium, in a silicate matrix dominated by silicon and aluminium with several per cent each of potassium and iron. Every figure is a mass fraction of the solid as the source reports it.
- assertion basis: SUBJECT_MEASURED
Evidence support: Supported by the cited evidence one source
Evidence: Jitka 2009 Primary authority